Now: Product Polyurethane paint

Polyurethane thick paste interpenetrating network anti-corrosion coating

Suitable for underground pipelines, including underground and submerged structures buried in various soil conditions, dock steel piles, etc.





Feedback > Contact >
  • Content
  • Application
  • Parameters
Construction precautions
1. The product should be stored in a cool, ventilated, and dry place, isolated from sources of fire, and kept away from heat sources.
2. This product is a thick paste coating, which can be applied with a thick coating without sagging. After opening the bucket, it can generally be brushed without adding diluent.
3. After the coating has been stored for too long, there may be slight precipitation, and it should be stirred before use.
4. After the coating is prepared, it should be heated for 20 minutes in summer and cured for 1-2 hours in winter before application. Generally, it should be used up within 8 hours, otherwise the viscosity will thicken and it will be difficult to apply.
5. After the primer surface dries, the topcoat can be applied. The interval at room temperature should not exceed two days, otherwise it will affect the interlayer bonding. The time gap between applying each layer of topcoat should also be based on surface dryness.